Strengthening of veneers for 3D-forming. 3D - forming of veneers is used only in limited extent. The reasons are wood properties, mainly anisotropy of wood. In this paper, we propose some chosen methods for strengthening of veneers in directions parallel and perpendicular to the grains, with strengthening means such as hotmelt adhesive and glass fibre with adhesive coating. Properties of modified veneers were compared with the properties of reference - untreated veneers. We compared these properties: strength and deformations - extension in tension, strength and deflection in bending, and 3D - formability. From the results, we can conclude that referred treatments resulted in a slight improvement of 3D - formability.
PL
Wzmacnianie fornirów do formowania 3D. Forniry charakteryzuje ograniczona formowalność. Przyczyną tego są własności drewna, głównie anizotropia. Praca prezentuje wybrane sposoby wzmacniania fornirów w kierunku poprzecznym i prostopadłym do włókien, za pomocą klejów topliwych i samoprzylepnych mat szklanych. Zbadano własności takich wzmocnionych fornirów z fornirami niemodyfikowanymi. Porównano wytrzymałość i elastyczność w rozciąganiu, zginaniu oraz formowalność 3D.

Słowa kluczowe

Wydawca

-

Rocznik

Tom

88

Opis fizyczny

p.297-303,fig.,ref.

Twórcy

autor
  • Department of Furniture and Wood Products, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T.G. Masaryka 24, 960 53 Zvolen, Slovakia
autor
  • Department of Furniture and Wood Products, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T.G. Masaryka 24, 960 53 Zvolen, Slovakia
autor
  • Department of Furniture and Wood Products, Faculty of Wood Sciences and Technology, Technical University in Zvolen, T.G. Masaryka 24, 960 53 Zvolen, Slovakia

Bibliografia

  • 1. BUCHELT B., WAGENFÜHR A., WENK S., 2009: 3-D-Beschichtung mit Furnier. HOB 3, p. 108-112.
  • 2. HUBER R., REINHARD H., 2007: Dreidimensional verformten Furnier im Trend, aber..... Informationsbedauf über Grundlagen der der Verarheitung und Anwendung. HK 1, p. 50 - 53
  • 3. LANGOVÁ N., JOŠČÁK P., MOŽUCHOVÁ M., TRENČANOVÁ L., 2013: Analysis the effects bending load of veneers for purposes of planar moulding. In: Annals of Warsaw University of Life Sciences. Forestry and wood technology. - No. 83, p. 173-178 ISSN 1898-5912.
  • 4. SCHULZ, T., SCHEIDING W., FISCHER M., 2012: Sperrholz und Sperrholzformteile aus thermisch modifizierten Furnieren. Holztechnologie 53, p.14-24.
  • 5. SLABEJOVÁ G., ŠMIDRIAKOVÁ M., 2013: Properties of modified veneers for 3 D - forming/ Gabriela Slabejová, Mária Šmidriaková. - VEGA 1/0422/12. In: Annals of Warsaw University of Life Sciences. Forestry and Wood Technology. - Warszawa : Warszaw University of Life Sciences Press, 2013. - ISSN 1898-5912. - No. 81 (2013), p. 248-252.
  • 6. SLABEJOVÁ G., ŠMIDRIAKOVÁ M., 2013: Influence of resin coating on strength and tensile deformation of beech veneer/ Gabriela Slabejová, Mária Šmidriaková. - VEGA 1/0422/12. In: Annals of Warsaw University of Life Sciences. Forestry and Wood Technology. - Warszawa : Warszaw University of Life Sciences Press, 2013.-ISSN 1898-5912. - No. 84 (2013), p. 186-189.
  • 7. VORREITER L., 1949: Holztechnologisches Handbuch, Band 1: Allgemeines, Holzkunde, Holzschutz und Holzvergütung. Verlag Georg Fromme & CO., Wien V, 1949, 548 p.
  • 8. WAGENFÜHR A., BUCHELT B., PFRIEM A., 2006: Material behaviour of veneer during multi dimensional moulding. In: Holz als Roh- und Werkstoff. [Online] 2006. [Dátum: 08. 01 2014.] č. 64, s. 83 - 89. Dostupné na internete: http://link.springer.com/article/10.1007/s00107-005-0008-5#page-1.

Typ dokumentu

Bibliografia

Identyfikatory

Identyfikator YADDA

bwmeta1.element.agro-cccd685c-af4d-4930-a3dc-3737d61349b0
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.